Heat Resistant Cast Steel Crank Arm For Walking Beam Furnace

Heat Resistant Cast Steel Crank Arm For Walking Beam Furnace

Failure Mode 01: Pin Bore Ovalization An undersized or improperly heat-treated bore deforms under oscillating load. Contact stress concentrates, wear accelerates, and the entire linkage misaligns - transferring additional bending moment into the arm body. Bores are machined after heat treatment,...
Send Inquiry
Description

b0f107d8aef9236ee72bd1a574be905c

117

Failure Mode 01: Pin Bore Ovalization

 

An undersized or improperly heat-treated bore deforms under oscillating load. Contact stress concentrates, wear accelerates, and the entire linkage misaligns - transferring additional bending moment into the arm body.

  • Bores are machinedafterheat treatment, not before.
  • Final geometry verified - not a pre-treatment dimension that shifts during cooling.
  • Roundness and taper checked against your drawing datums.

Failure Mode 02: Hub-to-Arm Fatigue

 

The arm and hub operate at different thermal masses. Repeated heating and cooling generates alternating stress at the transition. Shrinkage porosity or an unfavourable as-cast microstructure in that zone gives a fatigue crack its initiation point.

  • Critical section inspected with wall-thickness verification.
  • Surface integrity checks (Visual + PT) at the highest stress zone.
  • Solution annealing documented per heat number to stabilize the matrix.
116
The engineering decision that determines life.

The most expensive crank arm is not the one with the highest alloy content - it is the one that fails prematurely because the grade was selected for price rather than for the actual failure driver.

 
 

HH Grade

25Cr - 12Ni

Moderate temperature, higher thermal cycling frequency.

Furnace operates in the lower heating zone and cycle frequency dominates.
 



Baseline Cost

 
 
 

HK Grade

25Cr - 20Ni

Higher temperature with mixed oxidizing / sulphidizing atmosphere.

Crank arm sees sustained temperatures where HH would
 


 

scale or creep.

 
 
 

HN Grade

20Cr - 25Ni

Highest temperature, most severe thermal cycling.

Upper end of the walking beam window; outage cost justifies material premium.

 


Highest Cost

 

Every value tied to a heat number.

Production specifications, not catalogue ranges. All test reports and certificates ship with the casting.

Material Standard ASTM A297/A297M heat-resistant castings
Available Grades HH (25Cr-12Ni) · HK (25Cr-20Ni) · HN (20Cr-25Ni)
Service Temperature HH: up to 1050°C · HK: up to 1100°C · HN: up to 1150°C
Melting Electric-induction furnace
Casting Process Sand casting / Investment casting
Heat Treatment Solution annealing, documented time-temperature cycle per heat number
Bore Finishing Machined after heat treatment to final tolerance
Critical Inspection Hub-to-arm transition: wall-thickness + surface integrity (PT)
Hardness Report Reported per heat number against grade specification
Chemical Composition C, Mn, Si, P, S, Cr, Ni, Mo reported against ASTM A297
Documentation MTC, heat treatment chart, dimensional report, NDT (PT/UT)

Send your drawing. Get a spec-matched quote in 48 hours.

 

The more linkage and operating data you provide, the tighter the quote.

 

Crank arm drawing (PDF / DWG / STEP)

If no drawing: pin bore distance, arm angle, hub bore

Operating temperature (continuous and peak)

Walking beam mechanism type and cycle frequency

Material grade preference or operating envelope

modular-1
Contact us

 

 

Hot Tags: heat resistant cast steel crank arm for walking beam furnace, China heat resistant cast steel crank arm for walking beam furnace manufacturers, suppliers, factory, boiler parts, boiler sections, heat resistant steel casting parts, Integrally Cast Annealing Process Furnace Frame, parts in a boiler, parts of a boiler

Send Inquiry