Wear- And Corrosion-resistant Integrally Cast Spiral Auger

Wear- And Corrosion-resistant Integrally Cast Spiral Auger

Why is Integral Casting the Superior Choice for Screw Conveyors? When conveying highly abrasive materials (such as quartz sand, iron powder, coke slag, or coal gangue), the outer edge of traditional welded flights is often the weakest point prone to rapid wear. Integral casting fundamentally...
Send Inquiry
Description

5c530a2434a95a45c58937396d7f9b80

db71dad0e01bf9ff7f7ef10d69203d9d

Why is Integral Casting the Superior Choice for Screw Conveyors?

When conveying highly abrasive materials (such as quartz sand, iron powder, coke slag, or coal gangue), the outer edge of traditional welded flights is often the weakest point prone to rapid wear. Integral casting fundamentally eradicates this issue structurally.

 
 

Weldless Structure, Eliminates Fracture Risks

The flight and the central shaft are cast as a single piece, eliminating the Heat-Affected Zone (HAZ) and residual stress from welding. Under high-torque and high-impact conditions, it prevents flight tearing or detachment caused by weld seam cracking.

 
 
 

High-Chromium Carbides, Superior Abrasion Resistance

Made of Cr15-Cr28 high-chromium white cast iron, the matrix is dispersed with extremely hard M7C3 type chromium carbides (HV 1100-1600). This microstructure provides wear performance far exceeding standard wear-resistant steels in sliding abrasion applications.

 
 
 

No Hardfacing, Reduces Downtime Costs

Ready to install out of the box, eliminating the need for periodic hardfacing maintenance required by standard carbon steel flights. One installation provides months or even years of continuous, stable operation, significantly boosting Overall Equipment Effectiveness (OEE).

 

4e7760dff1f0c862113d1f3459087643

Manufacturing Capabilities & Material Standards

We support 1:1 custom manufacturing based on your original dimensions. Whether it's a standard pitch, variable pitch, or variable diameter design, we can achieve precise forming through 3D modeling and casting simulation.

 

✓ Custom to drawings / Reverse engineering from worn parts

✓ 3D casting simulation analysis report provided

✓ Shipped with Material Test Certificate (MTC) & Dynamic Balancing Report

Material Standard

 

High-Chromium White Cast Iron (Ref: ASTM A532 / GB/T 8263)

Chromium (Cr) Content

Cr 15% - 28% (Adjustable based on working conditions)

Hardness Range

 

HRC 58 - 65 (Depending on specific grade and heat treatment)

Outer Diameter Range

Φ 100 mm - Φ 2000 mm

Total Length

 

Max 6000 mm (Longer lengths via segmented casting and flange connection)

Casting Process

 

Lost Foam Casting (LFC) / Sand Casting / Centrifugal Casting

Full In-House Control from Pattern to Finished Product.

 

Casting high-chromium white iron is highly challenging; shrinkage during cooling and crack sensitivity require extreme process control. With mature Lost Foam and heat treatment lines, we ensure the yield and consistency of every pour.

 
01
 

Lost Foam Casting (LFC) Precision Forming

For complex spiral surfaces, vacuum Lost Foam casting significantly improves flight thickness uniformity, ensuring smooth material flow and reducing friction resistance.

 
02
 

Strict Heat Treatment & Stress Relief

As-cast high-chromium iron is brittle. Through controlled heating and cooling curves for stress-relief annealing or hardening, we maintain high hardness while providing the matrix with necessary toughness to resist impact.

 
03
 

Machining & Dynamic Balancing

Flanges and shaft bores are precision-machined to ensure assembly accuracy with the gearbox. For high-speed rotation applications, dynamic balancing tests are provided to reduce bearing loads and equipment vibration.

113
For Highly Abrasive Material Handling
 

Especially suitable for processes where material hardness and sharp particles cause rapid wear to standard metal flights.

Mining & Metallurgy

Conveying highly abrasive bulk materials like iron concentrate, sinter, coke slag, and quartz sand.

Brick & Ceramics

Vacuum extruder augers, heavy-duty extrusion of raw materials like coal gangue, shale, and fly ash.

Power & Environmental

Ash conveying systems in power plants, FGD limestone slurry transport, and sludge/solid waste handling.

Everything You Need to Know
 

High-chromium iron is known to be brittle. Will an integrally cast auger fracture during operation?

High-chromium white cast iron indeed has high hardness, with lower toughness compared to low-carbon steel. Therefore, our design premise is that the screw auger primarily endures abrasive wear rather than extreme high-impact loads. For conditions involving heavy particle impact, we can adjust the alloy formulation (e.g., adding Mo, Cu, Ni) or use a bi-metal composite process to enhance impact resistance while maintaining wear resistance. Please be sure to inform us of the maximum particle size and hardness during the inquiry.

Can you manufacture a 1:1 replacement based on my existing fabricated auger dimensions?

Absolutely. Simply provide your original equipment drawings (DWG/PDF/STEP) or send us a worn-out auger sample. Our engineers will use 3D scanning or physical mapping to recreate the casting model, ensuring that all installation dimensions (including center bore, flange hole spacing, pitch, and rotation direction) perfectly match your gearbox output shaft.

What is the lead time for integrally cast augers?

Since custom foam patterns or wooden molds must be made, the lead time for standard custom augers is approximately 25-35 days. For large augers with diameters exceeding 800mm or lengths over 3000mm, the schedule is evaluated based on specific process complexity. We will provide detailed inspection photos and videos after pouring, heat treatment, and machining are completed.

Why is integral casting more cost-effective than standard hardfaced flights?

While hardfaced carbon steel flights may have a lower initial unit price, their effective wear layer is only a few millimeters thick. Once worn through, the soft base metal fails rapidly, requiring frequent downtime for manual welding. Although the upfront cost of an integrally cast high-Cr auger is higher, its entire cross-section is wear-resistant, providing a lifespan 5-10 times longer. This eliminates significant downtime and labor costs, resulting in a much lower Total Cost of Ownership (TCO).

 

 

 

 

 

Hot Tags: wear- and corrosion-resistant integrally cast spiral auger, China wear- and corrosion-resistant integrally cast spiral auger manufacturers, suppliers, factory, boiler parts, heat resistant steel casting parts, Integrally Cast Annealing Process Furnace Frame, parts in a boiler, parts of a boiler, system boiler components