What this beam actually does in your furnace
The walking beam is not a static refractory support. Every cycle it lifts a full billet or slab load, translates it forward, and sets it down - under furnace atmosphere, at 950–1050 °C, thousands of times per campaign.
The failure modes that decide your maintenance interval are creep sag, thermal-fatigue cracking at section changes, and oxidation / carburization wall loss. ZG40Cr25Ni20 (2520 / HK40) is the grade specified when those three mechanisms define the replacement cycle.
Creep Sag
Long-duration load at temperature bows the beam and disturbs billet tracking in the discharge zone.
Thermal-Fatigue Cracking
Repeated stepping cycles crack fillets and section transitions - the classic failure point on cast beams.
Oxidation & Scaling
Cr–Si oxide film slows wall-thickness loss in oxidizing and mild carburizing atmospheres.
Verify this against your furnace builder's datasheet
| Parameter | ZG40Cr25Ni20 (2520) | Cross-reference |
| C | 0.35–0.45 % | ASTM A297 HK40 |
| Cr | 24–26 % | DIN 1.4848 |
| Ni | 19–21 % | GX40CrNiSi25-20 |
| Si | 1.5–2.5 % | - |
| Mn/P/S | Mn ≤ 1.5; P/S ≤ 0.04 % | - |
| Microstructure | Austenitic - no α↔γ transformation | Dimensionally stable under cycling |
| Long-term service | 950–1050 °C (some duties to 1100 °C) | Short-term peak 1150–1200 °C |
- Third-party inspection (SGS / BV / TPI) and heat-by-heat certificates available on request.
2520 sits at the workhorse position in the 25Cr-20Ni family. It offers well-proven oxidation resistance and thermal-shock tolerance at lower cost than high-Ni/W upgrades (e.g. 2848), and it is the default choice for preheat and heating-zone load-bearing beams, light-to-medium skid rails, and support blocks under cobalt-alloy skid buttons.
Soaking zone at sustained ≥ 1150 °C with heavy load?
Tell us - we will quote 2848 or another grade with the trade-off stated clearly. We do not push 2520 into a duty it was not designed for.
Performance points that show up in maintenance KPIs
Not lab adjectives - the mechanisms your maintenance planner can measure.
Creep resistance at temperature
The high-carbon austenitic matrix retains structural rigidity under long-duration 950–1050 °C exposure, resisting beam sag and bowing under billet load.
Thermal fatigue under cyclic stepping
The stepping motion imposes repeated thermal-mechanical cycles. 2520's single-phase structure avoids phase-change dimensional instability and reduces fillet cracking.
Oxidation & furnace-gas corrosion
The Cr–Si combination forms a protective oxide film that slows scaling and material loss in oxidizing and mild carburizing atmospheres.
Reproducibility from drawing to part
Precision sand casting or lost-wax casting + solution heat treatment, then CNC machining on mounting faces and interfaces for fit with the furnace support and drive.
Walking beams are not catalogue parts
We quote against your drawing, 3D model, or operating-condition parameters. Typical scope of supply:
Moving beam
Fixed beam
Water-cooled beam
Skid beam
Support beam
Tooth-type or plain top profile
Reinforced rib structure
Installation lug bosses
Water-cooled inner channel
Skid buttons / skid blocks
Replacing an imported beam or reverse-engineering an obsolete drawing? Send the original grade and key dimensions - we will confirm the 2520 equivalence and flag any section where a geometry change is advisable for castability or thermal fatigue.
What is checked before the beam ships
Chemical composition
Verified per heat against the 2520 specification listed above.
Solution heat treatment
Recorded and traceable to the individual part number.
Dimensional inspection
Mounting faces, lug bore spacing, and beam straightness - critical for stepping alignment.
Visual & surface inspection
Cast surfaces checked; machining marks and foundry marks documented.
Third-party inspection
SGS / BV / TPI available on request for EPC and steel-plant QA requirements.
Packing & marking
Heat number, part ID, and match-marking for on-site installation sequence.
Frequently Asked Questions
Is ZG40Cr25Ni20 the same as HK40 and 1.4848?
-
Yes for practical procurement purposes. ZG40Cr25Ni20 is the Chinese designation; HK40 is the ASTM A297 grade; 1.4848 / GX40CrNiSi25-20 is the DIN / EN equivalent. Minor Si ranges differ between standards - confirm the Si window on your datasheet if the part goes into a carburizing duty.
Can you supply the beam with skid buttons already fitted?
-
Yes. We supply 2520 beams with matching skid buttons / blocks, or with cobalt-alloy buttons where the wear duty requires an upgrade. Buttons can be cast, welded, or mechanically fastened per your drawing.
What drawing information do you need to quote?
-
Five items:
(1) overall length and cross-section;
(2) top profile / tooth geometry;
(3) mounting lug positions and bore sizes;
(4) water-cooling channel routing if applicable;
(5) operating temperature and load per beam.
A marked-up PDF or STEP file is sufficient for a first quotation.
What is the typical lead time?
-
For a new pattern: pattern-making + casting + heat treatment + machining, typically 6–9 weeks depending on size and quantity. Repeat orders with an existing pattern are shorter.
State your project milestone and we will confirm against foundry capacity.
Do you supply for both new furnace projects and maintenance replacement?
-
Both. We work with furnace OEMs and EPC contractors on new walking-beam furnace builds, and with steel-plant maintenance teams on campaign replacement.
For maintenance orders the priority is dimensional match to the existing installed beam - send photos and key measurements if the original drawing is unavailable.
Hot Tags: zg40cr25ni20 (2520) heat-resistant cast steel walking beam for reheating furnace, China zg40cr25ni20 (2520) heat-resistant cast steel walking beam for reheating furnace manufacturers, suppliers, factory, 310S Vacuum Furnace Charging Basket, boiler parts, boiler sections, heat resistant steel casting parts, Integrally Cast Annealing Process Furnace Frame, parts in a boiler